MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Abatron L060330-2 Flexible Polyurea Compound
Categories: Polymer; Adhesive; Thermoset

Material Notes: L060330-2 is used for castings, repairs, assemblies, coatings, and laminations that require fast hardening. It is also used for bonding most rigid materials such as metals, aluminum, copper, china, ceramic, glass, marble, wood fiberglass, leather, hard plastics, and electrical components. Other applications include traffic marker installation, roof patching, and concrete crack and joint filling. As it hardens even at freezing temperatures, it is widely used for installations, repairs, and maintenance in extremely cold environments. It characteristics include: curing time of 1-10 minutes, excellent adhesion without primer, excellent weather and water resistance, low temperature cure to -20°F, good thermal resistance to 300°F and excellent thermal cycling resistance, and useful in areas that are continually wet. L060330-2 is supplied in a two-component "caulking gun" system for minor repairs, holes, and filling, or professionally installed with a high pressure two-component mixing apparatus. It can also be in-line blended utilizing a two-component mixer/sprayer apparatus or a hand-held plural component caulking gun allowing the applicator to use amounts ranging from a few ounces to nearly continuous feed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Elongation at Break 400 %400 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -59.4 °C-75.0 °F
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 - 10.0 min0.0167 - 0.167 hour
Shelf Life 12.0 Month
@Temperature <=26.7 °C
12.0 Month
@Temperature <=80.0 °F
 
Descriptive Properties
Set Time (min)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion
CHT Group EP EF EPI Engineered Polymers Extra Flex Polyurea
CHT Group ReactAmine® EP 350 EPI Engineered Polymers Polyurea
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
Phillips 66 Polyurea NLGI Grade No. 1

PABC808 / 107792

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.