MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Dyflor® LE PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Thermoplastic, low viscosity plastic resin for injection molding, compression molding and extrusion.

Applications: Wire and cable jacketing.

ISO data as provided by the manufacturer.

Key Words: Polyvinylidinefluoride; Polyvinylidine Fluoride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³
Water Absorption 0.00 %0.00 %
Melt Flow 15 g/10 min15 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 8.0 %8.0 %
Modulus of Elasticity 2.10 GPa305 ksi
Charpy Impact Unnotched 26.0 J/cm²124 ft-lb/in²
 21.0 J/cm²
@Temperature -30.0 °C
99.9 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Tensile Impact Strength 140 kJ/m²66.6 ft-lb/in²
Tensile Creep Modulus, 1 hour 1600 MPa232000 psi
Tensile Creep Modulus, 1000 hours 950 MPa138000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  8.0
@Frequency 1e+6 Hz
8.0
@Frequency 1e+6 Hz
 9.0
@Frequency 100 Hz
9.0
@Frequency 100 Hz
Dielectric Strength 22.0 kV/mm559 kV/in
Dissipation Factor  0.034
@Frequency 100 Hz
0.034
@Frequency 100 Hz
 0.24
@Frequency 1e+6 Hz
0.24
@Frequency 1e+6 Hz
Comparative Tracking Index 275 V275 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °F
Vicat Softening Point 166 °C331 °F50°C/hr/50 N
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber
Evonik Dyflor® ME PVDF
Evonik Dyflor® EE PVDF
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK Extruded Unfilled Polyetherether Ketone
Kureha KF Polymer 850 PVDF Homopolymer

PHUL01 / 47261

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.