MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Dyflor® ME PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Thermoplastic, high viscosity plastic resin for injection molding, compression molding and extrusion.

Applications: Chemical facilities, machinery and vehicle construction, cable industry.

ISO data as provided by the manufacturer.

Key Words: Polyvinylidinefluoride; Polyvinylidine Fluoride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³
Water Absorption 0.00 %0.00 %
Melt Flow 2.0 g/10 min2.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 9.0 %9.0 %
Modulus of Elasticity 2.10 GPa305 ksi
Charpy Impact Unnotched NBNB
 26.0 J/cm²
@Temperature -30.0 °C
124 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 3.20 J/cm²15.2 ft-lb/in²
 1.10 J/cm²
@Temperature -30.0 °C
5.24 ft-lb/in²
@Temperature -22.0 °F
Tensile Impact Strength 210 kJ/m²99.9 ft-lb/in²
Tensile Creep Modulus, 1 hour 1150 MPa167000 psi
Tensile Creep Modulus, 1000 hours 900 MPa131000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.00e+12 ohm-cm8.00e+12 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  8.0
@Frequency 1e+6 Hz
8.0
@Frequency 1e+6 Hz
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
Dielectric Strength 19.0 kV/mm483 kV/in
Dissipation Factor  0.032
@Frequency 100 Hz
0.032
@Frequency 100 Hz
 0.25
@Frequency 1e+6 Hz
0.25
@Frequency 1e+6 Hz
Comparative Tracking Index 250 V250 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °F
Vicat Softening Point 166 °C331 °F50°C/hr/50 N
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber
Evonik Dyflor® EE PVDF
Evonik Dyflor® LE PVDF
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

PHUL02 / 47262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.