MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman DuraGrip™ 6160 BK Melt Processable Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel and will Bond to Nylon, ABS, PC, PC/ABS. DuraGrip™ 6100 series is hygroscopic and requires drying prior to use.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D471; ISO 2781
Viscosity 354000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
354000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 0.016 cm/cm0.016 in/in
Linear Mold Shrinkage, Transverse 0.00 cm/cm0.00 in/in
 0.0050 cm/cm0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 6.62 MPa960 psiASTM D412; ISO 37
 7.3457 MPa1065.4 psiAfter 7 days at 70°C; ASTM D412 ISO 37
 9.267 MPa1344 psiAfter 7 days at 100°C; ASTM D412 ISO 37
Elongation at Break 350 %350 %ASTM D412; ISO 37
 364 %364 %After 7 days at 70°C; ASTM D412 ISO 37
 413 %413 %After 7 days at 100°C; ASTM D412 ISO 37
Modulus of Elasticity 0.00210 GPa0.304 ksiAfter 7 days at 100°C; ASTM D412 ISO 37
 0.00225 GPa0.326 ksiAfter 7 days at 70°C; ASTM D412 ISO 37
100% Modulus 2.21 MPa
@Strain 100 %
320 psi
@Strain 100 %
ASTM D412; ISO 37
Graves Tear Strength 29.5 kN/m
@Temperature 23.9 °C
168 pli
@Temperature 75.0 °F
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 189189Cs-17 Wheel, 1000 g Load; ASTM D3389
Compression Set  82 %
@Temperature 70.0 °C
82 %
@Temperature 158 °F
22 hrs.; ASTM D395; ISO 815
 91 %
@Temperature 100 °C
91 %
@Temperature 212 °F
22 hrs.; ASTM D395; ISO 815
 21 %
@Temperature 24.0 °C,
Time 79200 sec
21 %
@Temperature 75.2 °F,
Time 22.0 hour
ASTM D395; ISO 815
Tensile Set 4.1 %4.1 %100% Tension; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -65.0 °C-85.0 °FASTM D746; ISO 812
 
Processing PropertiesMetricEnglishComments
Processing Temperature 227 °C440 °F
Rear Barrel Temperature 204 - 221 °C400 - 430 °F
Middle Barrel Temperature 216 - 227 °C420 - 440 °F
Front Barrel Temperature 227 - 238 °C440 - 460 °F
Nozzle Temperature 227 - 249 °C440 - 480 °F
Melt Temperature 227 - 254 °C440 - 490 °F
Mold Temperature 43.3 - 54.4 °C110 - 130 °F
Injection Pressure 1.03 - 3.45 MPa150 - 500 psi
Cycle Time - Injection 0.50 - 2.0 sec0.50 - 2.0 secboost
Screw Speed 25 - 100 rpm25 - 100 rpm
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourCooling Time
 
Descriptive Properties
Fluid Resistance - Volume Change, % (ASTM D471)12After 7 Days in ASTM Oil No.1 at 212°F (100°C)
 2After 7 Days in Water at 212°F (100°C)
 52After 7 Days in ASTM Ref. Fuel No. B at 75°F (24°C)
 74After 7 Days in IRM 903 Oil No.3 at 212°F (100°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6170 NC Thermoplastic Elastomer (TPE)
6160 Aluminum Composition Spec
Aluminum 6061-O
A. Schulman DuraGrip™ 6170 BK Melt Processable Elastomer

PAPA044 / 24111

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.