MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman DuraGrip™ DGR 6170 NC Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: DuraGrip® DGR 6170 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylon, ASA, PC/ABS alloys, PBT, and PC/PBT alloys. It is easy to use in injection molding and extrusion processes. DGR 6170NC has excellent elastomeric properties and soft touch feel. DuraGrip® bonding grades are hygroscopic, and for best results drying is recommended prior to use.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D471
Viscosity 420000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
420000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 68685 Sec; ASTM D2240
Tensile Strength at Break 9.198 MPa1334 psiASTM D412
Elongation at Break 420 %420 %ASTM D412
100% Modulus 2.80 MPa
@Strain 100 %
406 psi
@Strain 100 %
ASTM D412
Graves Tear Strength 43.8 kN/m
@Temperature 24.0 °C
250 pli
@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 22 %
@Temperature 24.0 °C,
Time 79200 sec
22 %
@Temperature 75.2 °F,
Time 22.0 hour
ASTM D395
Tensile Set 5.0 %5.0 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -65.0 °C-85.0 °FASTM D746
 
Descriptive Properties
ColorN,B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 6003-55A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ 6160 BK Melt Processable Elastomer
A. Schulman DuraGrip™ 6170 BK Melt Processable Elastomer
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested

PAPA042 / 24109

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.