MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kao-Tuff 110C Castables
Categories: Ceramic; Oxide

Material Notes: Kao-Tuff 110C is a medium-weight erosion-resistant castable with excellent insulating properties. Abrasion losses 8 - 15 cc’s and a thermal conductivity of 5.5 at 1500°F (816°C) make it effective for numerous applications in F.C.C.U. and other industrial uses.

Features:

  • Feature specially enhanced properties that allow them to outperform conventional refractories
  • Abrasion losses from 8 to 22 cc’s
  • Gunning, hand packing and cast vibration placement techniques
  • Applications:

  • FCCU
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.667 - 1.827 g/cc0.06022 - 0.06600 lb/in³Fired at 1500°F
     1.683 - 1.811 g/cc0.06080 - 0.06543 lb/in³Fired at 2400°F
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00827 - 0.0124 GPa1.20 - 1.80 ksiDried 18-24 hours at 220°F; ASTM C133
     0.00552 - 0.00724 GPa
    @Treatment Temp. 816 °C,
    Time 18000 sec
    0.800 - 1.05 ksi
    @Treatment Temp. 1500 °F,
    Time 5.00 hour
    ASTM C133
     0.00552 - 0.00827 GPa
    @Treatment Temp. 1260 °C,
    Time 18000 sec
    0.800 - 1.20 ksi
    @Treatment Temp. 2300 °F,
    Time 5.00 hour
    ASTM C133
    Compressive Strength 37.9 - 58.6 MPa5500 - 8500 psiFired 5 hours at 1500°F; ASTM C133
     41.4 - 62.1 MPa6000 - 9010 psiDried for 18-24 hours at 220°F
     45.5 - 62.1 MPa6600 - 9010 psiFired 5 hours at 2400°F
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.778 W/m-K
    @Temperature 260 °C
    5.40 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C417
     0.778 W/m-K
    @Temperature 538 °C
    5.40 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C417
     0.793 W/m-K
    @Temperature 816 °C
    5.50 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C417
     0.821 W/m-K
    @Temperature 1090 °C
    5.70 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C417
    Maximum Service Temperature, Air 1320 °C2400 °F
    Shrinkage  -0.400 - 0.40 %
    @Temperature 1320 °C,
    Time 18000 sec
    -0.400 - 0.40 %
    @Temperature 2400 °F,
    Time 5.00 hour
    ASTM C113
     0.10 - 0.40 %
    @Temperature 816 °C,
    Time 18000 sec
    0.10 - 0.40 %
    @Temperature 1500 °F,
    Time 5.00 hour
    ASTM C113
     0.00 - 0.20 %
    @Treatment Temp. 104 °C
    0.00 - 0.20 %
    @Treatment Temp. 220 °F
    Dried 18-24 hours; ASTM C113
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 12.0 Month12.0 Month
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 43 %43 %
    Alkalis 0.20 %0.20 %
    CaO 15 %15 %
    Fe2O3 1.8 %1.8 %
    MgO 0.40 %0.40 %
    SiO2 39 %39 %
    TiO2 0.70 %0.70 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Thermal Ceramics Kao-Tuff 110G Castables

    CTHERM065 / 2385

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.