MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro MULTRANOL® 3900 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Multranol 3900 polyether polyol is a 4,800-molecular-weight polyoxypropylene triol specially modified with ethylene oxide.

Properties / Applications Multranol 3900 polyether polyol is a 4,800-molecular-weight polyoxypropylene triol specially modified with ethylene oxide. The terminal end-groups have a high percentage of primary hydroxyl end-groups, giving it a relatively high rate of reactivity with isocyanates. It is compatible with most polyether polyols and can be blended with other diols, triols, and polymer polyols to achieve desirable modifications of product properties. Multranol 3900 polyol is used in a broad range of urethane foam and other applications, including sealants, caulks, deck coatings, elastomers, tire fill, and reaction injection molding (RIM). As with any product, the use of Multranol 3900 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Viscosity 820 cP820 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.015<= 0.015[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 184 °C363 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50PtCo
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0925 / 202708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.