- Formulated for inert-gas, metallic-arc, and/or gas welding of stainless steel, high chromium ferrous alloys, and low Nickel alloys.
- Provides significant protection and improves weld quality.
- Most cost-effective alternative for backside protection in lieu of Nitrogen, Argon, or other gases.
Superior No. 9 Welding Back–up Flux is formulated for Mig and Tig welding stainless steel and low nickel (less than 20%) heat resistant alloys. The flux prevents oxide inclusion formation, protects the backside from oxidation, supports the molten metal, and reduces burn-through. It is a more cost effective means of achieving backside protection than other alternatives, including back up bars, inert gas purge, back-up tape, and even other back-up fluxes. Additionally, the flux can be placed in areas where back-up bars or back-up tapes are impractical; such as parts with irregular shapes or bends.Information provided by Superior Flux |