MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 9 Welding Back-up Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Formulated for inert-gas, metallic-arc, and/or gas welding of stainless steel, high chromium ferrous alloys, and low Nickel alloys.
  • Provides significant protection and improves weld quality.
  • Most cost-effective alternative for backside protection in lieu of Nitrogen, Argon, or other gases.
Superior No. 9 Welding Back–up Flux is formulated for Mig and Tig welding stainless steel and low nickel (less than 20%) heat resistant alloys. The flux prevents oxide inclusion formation, protects the backside from oxidation, supports the molten metal, and reduces burn-through. It is a more cost effective means of achieving backside protection than other alternatives, including back up bars, inert gas purge, back-up tape, and even other back-up fluxes. Additionally, the flux can be placed in areas where back-up bars or back-up tapes are impractical; such as parts with irregular shapes or bends.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/cc
Volatiles <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1090 - 1540 °C1990 - 2800 °FActive Range
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
FormFine Gray Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® ASB-0670 Metal-Back Composite
Celanese Ateva® 2810A Ethylene Vinyl Acetate Copolymer
AISI 1020 Steel, cold rolled
3M 2515 Flat Back Paper Masking Tape

NSFLUX003 / 185687

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.