MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex ELEXAR® EL 8614 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Notes: Elexar® EL-8614 is high performance thermoplastic elastomer designed for a variety of electrical applications requiring flexibility over a wide temperature range. Elexar® EL-8614 is a high density, high hardness, halogenated, flame-retardant grade that is RoHS compliant. This grade is UL listed and is suitable for both injection molding and extrusion.

Features: Filled; Flame Retardant; Halogenated; High Density; High Hardness; High Specific Gravity; Low Flow

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Moisture Absorption at Equilibrium 3.3 %
@Temperature 80.0 °C
ASTM D570
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96
@Time 5.00 sec
ASTM D2240
Hardness, Shore D 54
@Time 5.00 sec
ASTM D2240
Tensile Strength, Yield 2240 psiASTM D412
 1836.8 psi
@Treatment Temp. 60.0 °C,
Time 605000 sec
in ASTM #2 Oil; ASTM D471
 1926.4 psi
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
Tensile Stress at Strain 922 psi
@Strain 100 %
ASTM D412
 1230 psi
@Strain 300 %
ASTM D412
Elongation at Break 570 %ASTM D412
 456 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 490.2 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in ASTM #2 Oil; ASTM D471
Tear Strength 380 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.20e+16 ohm-cmASTM D257
Surface Resistance 3.50e+16 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
ASTM D150
 2.34
@Frequency 60 Hz
ASTM D150
 2.8
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0020
@Frequency 60 Hz
ASTM D150
 0.0020
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °CContinuous; UL-1581
Brittleness Temperature -49.0 °CASTM D746
UL RTI, Electrical 194 °FUL 746
UL RTI, Mechanical with Impact 194 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
Natural Color
 V-2
@Thickness 3.05 mm
Natural Color
Oxygen Index 25 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 420 °F
Middle Barrel Temperature 415 - 430 °F
Front Barrel Temperature 430 - 440 °F
Nozzle Temperature 430 - 445 °F
Zone 1 380 - 410 °F
Zone 2 390 - 420 °F
Zone 3 415 - 430 °F
Zone 5 430 - 440 °F
Die Temperature 430 - 445 °F
Melt Temperature 430 - 445 °FProcessing Temp
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex ELEXAR® EL 8730 Thermoplastic Elastomer
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer
Teknor Apex Elexar® EL-8730A Thermoplastic Elastomer
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer

PTEKNO263 / 70006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.