Moplen EP140R is a medium fluidity heterophasic copolymer grade for injection molding applications. It exhibits an excellent impact performance, particularly at low temperature, combined with a good processability. Moplen EP140R is an ideal building block for technical compounding. It offers a good solution for interior and exterior parts in Automotive compounds. It is not intended for medical and pharmaceutical applications. The grade is available in natural, pellet form. Status: Developmental Availability: Africa-Middle East; Europe Application: Automotive Parts Market: Automotive Processing Method: Compounding; Injection Molding Attribute: Good Flow; High Impact Resistance Information provided by LyondellBasell. |