MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen EP140R Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP140R is a medium fluidity heterophasic copolymer grade for injection molding applications. It exhibits an excellent impact performance, particularly at low temperature, combined with a good processability. Moplen EP140R is an ideal building block for technical compounding. It offers a good solution for interior and exterior parts in Automotive compounds. It is not intended for medical and pharmaceutical applications. The grade is available in natural, pellet form.

Status: Developmental

Availability: Africa-Middle East; Europe

Application: Automotive Parts

Market: Automotive

Processing Method: Compounding; Injection Molding

Attribute: Good Flow; High Impact Resistance

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccISO 1183-1
Melt Flow 22.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPaISO 527-1, -2
Tensile Strength, Yield 13.0 MPaISO 527-1, -2
Elongation at Break 100 %ISO 527-1, -2
Elongation at Yield 7.00 %ISO 527-1, -2
Tensile Modulus 600 MPaISO 527-1, -2
Flexural Modulus 650 MPaISO 178
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 14.0 kJ/m²
@Temperature -20.0 °C
Type 1, Edgewise, Notch A; ISO 179
 30.0 kJ/m²
@Temperature 0.000 °C
ISO 179
 65.0 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 130 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9653 / 324588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.