MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool 3000 Paper
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minimum. This specialty paper is noted for its excellent flexibility, outstanding handling characteristics, and high insulating value at high temperatures.

Features:

  • High alumina, fiber index and purity
  • Outstanding high temperature stability
  • Thin, flexible, high temperature insulation
  • Easily die-cut to form complex shapes for high temperature gasketing
  • Conforms easily to complex shapes
  • Excellent high temperature parting agent
  • Excellent high temperature backup and expansion joint material
  • Applications:

  • High temperature gaskets and seals
  • Refractory back-up insulation
  • Appliance insulation
  • Separating media for heat treating metals
  • High temperature filtration
  • High temperature expansion joint packing
  • Glassware separating media
  • Parting agent for brazing operations
  • Hot face and backup lining for lab furnaces
  • Aluminum distributor pan lining
  • Super alloy ingot mold lining and hot tapes.
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.112 - 0.160 g/cc0.00405 - 0.00578 lb/in³
    Loss On Ignition 6.0 - 10 %6.0 - 10 %
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.0345 MPa5.00 psiFired
     0.172 - 0.276 MPa25.0 - 40.0 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0519 W/m-K
    @Temperature 260 °C
    0.360 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.0764 W/m-K
    @Temperature 538 °C
    0.530 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.115 W/m-K
    @Temperature 816 °C
    0.800 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.173 W/m-K
    @Temperature 1090 °C
    1.20 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
     0.256 W/m-K
    @Temperature 1370 °C
    1.78 BTU-in/hr-ft²-°F
    @Temperature 2500 °F
     0.320 W/m-K
    @Temperature 1540 °C
    2.22 BTU-in/hr-ft²-°F
    @Temperature 2800 °F
    Melting Point 1980 °C3600 °F
    Maximum Service Temperature, Air 1540 °C2800 °F
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 95 %95 %
    SiO2 5.0 %5.0 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Morgan Advanced Ceramics Kaowool HP Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
    Morgan Advanced Ceramics Kaowool C Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
    Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

    CTHERM245 / 2565

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.