Characterization: 10% glass fibers, mineral reinforced, medium viscosity, stabilized, qualified for LPKF LDS process, optimized shrinkage, suitable for lead-free solders. Partly biobased and eco-friendly Applications: Three-dimensional interconnect devices in electronic applications, specially adapted for the LDS process. Dimension-stable, glossy surface Information provided by Evonik |