MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals P453B Expandable Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for low and standard density foam.

Applications: Stryrocell P453B is used mainly for producing standard density block, which are subsequently cut to board for insulation or packaging.

This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs. Dutch Food Packaging Regulations. Recommendations of German Federal Office of Health (BGA), now regulated by the new Institute of Consumer Health (BGVV), Empfehlung V. US Food and Drug Administration Code of Federal Regulations title 21, sections 177.1640 (Polystyrene) and 178.3010 (Blowing Agents).

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density >= 0.0140 g/cc>= 0.000506 lb/in³Minimum achievable; Single stage per-expansion in continuous expander at atmospheric pressure
 0.0100 - 0.0200 g/cc0.000361 - 0.000723 lb/in³Normal molded density assuming cost optimized selection of processing conditions.
Bead Size 1.00 - 1.30 mm0.0394 - 0.0512 in
 0.710 - 1.70 mm0.0280 - 0.0669 inBerre Laboratory Analytical Methods 0492
 
Chemical PropertiesMetricEnglishComments
Styrene Content <= 0.10 %<= 0.10 %Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
Blowing Agent Content >= 6.1 %>= 6.1 %Berre Laboratory Analytical Methods 0076

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Expanded Polystyrene (EPS)
Overview of materials for Polyimide
NOVA Chemicals P163B Expandable Polystyrene
General Plastics LAST-A-FOAM® FP-8015 Foam
BASF Neopolen® P 9270 0.1 g/cc Core density; Expanded Polypropylene (Europe)

PNOVA336 / 55234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.