MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  60.0 MPa
@Temperature 120 °C
8700 psi
@Temperature 248 °F
 70.0 MPa
@Temperature 90.0 °C
10200 psi
@Temperature 194 °F
 85.0 MPa
@Temperature 60.0 °C
12300 psi
@Temperature 140 °F
 95.0 MPa
@Temperature 23.0 °C
13800 psi
@Temperature 73.4 °F
Elongation at Break  1.5 %
@Temperature 90.0 °C
1.5 %
@Temperature 194 °F
 1.5 %
@Temperature 120 °C
1.5 %
@Temperature 248 °F
 1.6 %
@Temperature 60.0 °C
1.6 %
@Temperature 140 °F
 1.8 %
@Temperature 23.0 °C
1.8 %
@Temperature 73.4 °F
Tensile Modulus  4.50 GPa
@Temperature 120 °C
653 ksi
@Temperature 248 °F
 5.70 GPa
@Temperature 90.0 °C
827 ksi
@Temperature 194 °F
 6.00 GPa
@Temperature 60.0 °C
870 ksi
@Temperature 140 °F
 6.50 GPa
@Temperature 23.0 °C
943 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 150 V150 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Vicat Softening Point 140 °C
@Load 5.00 kg
284 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 120 - 130 °C
@Time 10800 sec
248 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® HTNFR52G30BL NC010 PA6T/66-GF30FR(16+72)
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
PTS Tristar® PC-20GF 20% Glass Reinforced Polycarbonate
Mocom (ALBIS) ALTECH® PC ECO 2020/146 FR GF20 PC, 20% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PC ECO 2020/140 PC, 20% Glass Fiber Reinforced

PLATH9844 / 177540

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.