MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa
@Temperature 120 °C
 70.0 MPa
@Temperature 90.0 °C
 85.0 MPa
@Temperature 60.0 °C
 95.0 MPa
@Temperature 23.0 °C
Elongation at Break 1.5 %
@Temperature 90.0 °C
 1.5 %
@Temperature 120 °C
 1.6 %
@Temperature 60.0 °C
 1.8 %
@Temperature 23.0 °C
Tensile Modulus 4500 MPa
@Temperature 120 °C
 5700 MPa
@Temperature 90.0 °C
 6000 MPa
@Temperature 60.0 °C
 6500 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 40.0 kJ/m²
Charpy Impact, Notched 10.0 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 150 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
Vicat Softening Point 140 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
Mold Temperature 100 - 120 °C
Drying Temperature 120 - 130 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® HTNFR52G30BL NC010 PA6T/66-GF30FR(16+72)
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
PTS Tristar® PC-20GF 20% Glass Reinforced Polycarbonate
Mocom (ALBIS) ALTECH® PC ECO 2020/146 FR GF20 PC, 20% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PC ECO 2020/140 PC, 20% Glass Fiber Reinforced

PLATH9844 / 177540

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.