MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Larpeek 50 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Linear Mold Shrinkage, Flow 0.0085 - 0.0125 cm/cm0.0085 - 0.0125 in/in
Linear Mold Shrinkage, Transverse 0.0095 - 0.0135 cm/cm0.0095 - 0.0135 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  30.0 MPa
@Temperature 150 °C
4350 psi
@Temperature 302 °F
 50.0 MPa
@Temperature 120 °C
7250 psi
@Temperature 248 °F
 60.0 MPa
@Temperature 90.0 °C
8700 psi
@Temperature 194 °F
 75.0 MPa
@Temperature 60.0 °C
10900 psi
@Temperature 140 °F
 85.0 MPa
@Temperature 23.0 °C
12300 psi
@Temperature 73.4 °F
Elongation at Break  30 %
@Temperature 23.0 °C
30 %
@Temperature 73.4 °F
 30 %
@Temperature 60.0 °C
30 %
@Temperature 140 °F
 30 %
@Temperature 90.0 °C
30 %
@Temperature 194 °F
 35 %
@Temperature 120 °C
35 %
@Temperature 248 °F
 45 %
@Temperature 150 °C
45 %
@Temperature 302 °F
Elongation at Yield  5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
 5.0 %
@Temperature 60.0 °C
5.0 %
@Temperature 140 °F
 5.0 %
@Temperature 90.0 °C
5.0 %
@Temperature 194 °F
 6.0 %
@Temperature 120 °C
6.0 %
@Temperature 248 °F
 8.0 %
@Temperature 150 °C
8.0 %
@Temperature 302 °F
Tensile Modulus  3.00 GPa
@Temperature 150 °C
435 ksi
@Temperature 302 °F
 3.40 GPa
@Temperature 120 °C
493 ksi
@Temperature 248 °F
 3.45 GPa
@Temperature 90.0 °C
500 ksi
@Temperature 194 °F
 3.50 GPa
@Temperature 23.0 °C
508 ksi
@Temperature 73.4 °F
 3.50 GPa
@Temperature 60.0 °C
508 ksi
@Temperature 140 °F
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²
Coefficient of Friction, Dynamic 0.260.26
Coefficient of Friction, Static 0.320.32
K (wear) Factor 15.0 x 10-8 mm³/N-M7.45 x 10-10 in³-min/ft-lb-hr
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °F
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °F
Vicat Softening Point >= 300 °C
@Load 5.00 kg
>= 572 °F
@Load 11.0 lb
Flammability, UL94  V-1
@Thickness 0.750 mm
V-1
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
1610 °F
@Thickness 0.0394 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 360 - 390 °C680 - 734 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 120 - 150 °C
@Time 10800 sec
248 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
VICTREX™ PEEK 450G™ General Purpose
Overview of materials for Polyetheretherketone, Unreinforced
Lotte Advanced Materials Starex® HF-5661H ASA, Unreinforced

PLATH9645 / 177341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.