MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium LS141, Ultralight Mg-Li Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 20000 psi
Tensile Strength, Yield 16000 psi
Elongation at Break 23 %in 50 mm
Modulus of Elasticity 41.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000152 ohm-cmEstimated from similar Mg alloys
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.7 µm/m-°C
@Temperature 24.0 - 100 °C
estimated from similar Mg alloys
 22.2 µm/m-°C
@Temperature 100 - 200 °C
estimated from similar Mg alloys
Specific Heat Capacity 1.449 J/g-°CEstimated from similar Mg alloys
Thermal Conductivity 80.0 W/m-KEstimated from similar Mg alloys
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 - 0.80 %
Lithium, Li 13 - 15 %
Magnesium, Mg 84 - 86 %As Remainder

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium LA141, Ultralight Mg-Li Alloy
Magnesium AZ61A-F, Extruded Hollow Shapes
Magnesium AZ80A-T5, Extruded
Magnesium AZ61A-F, Forgings
Overview of materials for Beryllium Alloy

MMLS141 / 12453

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.