MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°C). The alloy also offers good resistance to sulfidation and resistance to wear and galling. Alloy L-605 is useful in gas turbine applications such as rings, blades and combustion chamber parts (sheet fabrications) and can also be used in industrial furnace applications such as mufflers or liners in high-temperature kilns.

Information Provided by Special Metals Corporation

Key Words: UNS R30605; AMS 5537, 5759, 5796, 5797
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 9.27 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 994 MPa
 150 MPa
@Temperature 1100 °C
 700 MPa
@Temperature 650 °C
 900 MPa
@Temperature 200 °C
Tensile Strength, Yield 466 MPa
 75.0 MPa
@Strain 0.2 %,
Temperature 1100 °C
 225 MPa
@Strain 0.2 %,
Temperature 650 °C
 400 MPa
@Strain 0.2 %,
Temperature 200 °C
Elongation at Break 50 %
 35 %
@Temperature 650 °C
 35 %
@Temperature 1100 °C
 60 %
@Temperature 200 °C
Rupture Strength 25.0 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
 44.0 MPa
@Temperature 927 °C,
Time 3.60e+6 sec
 72.0 MPa
@Temperature 871 °C,
Time 3.60e+6 sec
 120 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
 165 MPa
@Temperature 760 °C,
Time 3.60e+6 sec
 220 MPa
@Temperature 704 °C,
Time 3.60e+6 sec
 270 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 533.2 ohm-cir-mil/ft
@Temperature 24.0 °C
Magnetic Permeability 1.002at 200 Oersted
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.24 µin/in-°F
@Temperature 93.3 °C
 7.43 µin/in-°F
@Temperature 204 °C
 7.66 µin/in-°F
@Temperature 316 °C
 7.89 µin/in-°F
@Temperature 427 °C
 8.06 µin/in-°F
@Temperature 538 °C
 8.28 µin/in-°F
@Temperature 649 °C
 8.68 µin/in-°F
@Temperature 760 °C
 8.94 µin/in-°F
@Temperature 871 °C
Specific Heat Capacity 0.385 J/g-°C
@Temperature 21.0 °C
Thermal Conductivity 9.40 W/m-K
Melting Point 1330 - 1410 °C
Solidus 1330 °C
Liquidus 1410 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.050 - 0.15 %
Chromium, Cr 19 - 21 %
Cobalt, Co 46.38 - 56.95 %Balance
Iron, Fe <= 3.0 %
Manganese, Mn 1.0 - 2.0 %
Nickel, Ni 9.0 - 11 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.030 %
Tungsten, W 14 - 16 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Special Metals INCONEL® Alloy 625
Universal Wire Works Haynes 25 (L-605) (AMS 5796) Filler Metal
Aluminum 6061A Composition Spec

NINDA17 / 98908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.