MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Data provided by Allvac.

Applications: High temperature applications, jet engine components, devices in high fatigue service.

Key Words: Allvac, an Allegheny Teledyne Company, UNS R30605; AMS 5759. ASTM F 90
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.22 g/cc0.333 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080
Tensile Strength, Ultimate 1035 MPa150100 psi
Tensile Strength, Yield 414 MPa
@Strain 0.2 %
60000 psi
@Strain 0.2 %
Elongation at Break 60 %60 %
Reduction of Area 40 %40 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 20 %20 %
Cobalt, Co 53 %53 %
Iron, Fe 0.50 %0.50 %
Manganese, Mn 1.7 %1.7 %
Nickel, Ni 10 %10 %as balance
Tungsten, W 15 %15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
ATI Allvac® 35N Nickel Superalloy BIllet, Heat Treatment: 1052°C (1925°F) + Age
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Phynox Cobalt-Chromium-Nickel Alloy

NALL21 / 14789

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.