MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ampco Metal AMPCO® 18.136 Aluminum Bronze, Centrifugal
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: AMPCO 18.136 is a variation of AMPCO 18 specifically heat-treated to increase the impact resistance by 40% (see Charpy values) and the elastic limit in compression by 10 % without affecting the tensile strength of the alloy.

Applications: This AMPCO 18.136 has been tailor-made for steel mill applications as slippers and screw-down nuts and for similar applications where an extreme wear pressure is combined with important impact loading.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.45 g/cc0.269 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170HB 30
Hardness, Rockwell B 8787
Tensile Strength, Ultimate 689 MPa99900 psi
Tensile Strength, Yield 289 MPa
@Strain 0.5 %
41900 psi
@Strain 0.5 %
Elongation at Break 20 %20 %
Reduction of Area 20 %20 %
Modulus of Elasticity 110 GPa16000 ksi
Compressive Yield Strength 221 MPa32100 psiProportional Limit
Compressive Strength 979 MPa142000 psi
Fatigue Strength 214 MPa
@# of Cycles 1.00e+8
31000 psi
@# of Cycles 1.00e+8
Shear Strength 386 MPa56000 psi
Izod Impact 30.0 J22.1 ft-lb
Charpy Impact 22.0 J16.2 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000133 ohm-cm0.0000133 ohm-cm13% I.A.C.S.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
9.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 59.0 W/m-K409 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10.5 %10.5 %
Copper, Cu 85.5 - 86 %85.5 - 86 %As Balance
Iron, Fe 3.5 %3.5 %
Other, total <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S24100 Stainless Steel 25 mm annealed bar at RT
AISI Type 651 (19-9 DL) Stainless Steel warm worked and stress relieved
AISI Type 651 (19-9 DL) Stainless Steel cold drawn and stress relieved
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
ASTM A808 HSLA Steel, Thickness < 40 mm (1.5 in.)

NAMPCO12 / 14966

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.