MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility.

ELKALOY® D120 material is recommended for heavy-duty butt or flash welding jaws, clamps and dies. It is also used for machine parts to resist heavy pressure and extreme wear. It is a superior material as a guide bushing for automatic arc welders, heavy-duty bearings slides and gibbs when used in contact with steel.

Information provided by CMW Inc.

1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95
Tensile Strength, Ultimate 586 MPa
Tensile Strength, Yield 276 MPa
Elongation at Break 4.0 %
Reduction of Area 3.0 %
Modulus of Elasticity 97.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000172 ohm-cm10 % IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 71.0 W/m-K
Melting Point 1025 - 1060 °C
Solidus 1025 °C
Liquidus 1060 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 11.6 %
Beryllium, Be 0.50 %
Co + Ni 1.5 - 2.55 %
Copper, Cu 81.45 - 82.5 %
Iron, Fe 3.9 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® ELKALOY D Copper Alloy, Aluminum Bronze
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)
Cadi MOLD-MOR™ 3

NCMW074 / 15887

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.