MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Assab Steels ASP 30 Cold Work Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel

Material Notes: ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:
  • High wear resistance
  • High compressive strength at high hardness
  • Good through hardening properties
  • Good toughness
  • Good dimensional stability on heat treatment
  • Very good temper resistance

  • The combination of high wear resistance and unusually good compressive strength can be put to use in tooling for heavy forming operations.

W.-NR. 1.3207

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.287 lb/in³soft annealed condition
 0.284 lb/in³
@Temperature 600 °C
soft annealed condition
 0.285 lb/in³
@Temperature 400 °C
soft annealed condition
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 63
@Diameter 5.00 mm
Four point bend testing. 5mm/min. Austenitizing temperature: 1050°C Tempering: 3X1 h at 560°C, AC
 66
@Diameter 5.00 mm
Four point bend testing. 5mm/min. Austenitizing temperature: 1050°C Tempering: 3X1 h at 560°C, AC
Modulus of Elasticity 240 GPa
 192 GPa
@Temperature 400 °C
Flexural Strength 2000 MPaRmb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1250°C Tempering: 3X1 h at 560°C, AC
 3100 MPaReb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1100°C Tempering: 3X1 h at 560°C, AC
 4000 MPaReb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1200°C Tempering: 3X1 h at 560°C, AC
 4500 MPaRmb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1200°C Tempering: 3X1 h at 560°C, AC
 5500 MPaRmb. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 1100°C Tempering: 3X1 h at 560°C, AC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.8 µm/m-°C
@Temperature 20.0 - 400 °C
for the hardened and tempered condition
 12.3 µm/m-°C
@Temperature 20.0 - 600 °C
for the hardened and tempered condition
Specific Heat Capacity 0.100 BTU/lb-°F
@Temperature 20.0 °C
hardened and tempered condition
 0.120 BTU/lb-°F
@Temperature 400 °C
hardened and tempered condition
 0.140 BTU/lb-°F
@Temperature 600 °C
hardened and tempered condition
Thermal Conductivity 22.0 W/m-K
@Temperature 20.0 °C
hardened and tempered condition
 25.0 W/m-K
@Temperature 600 °C
hardened and tempered condition
 26.0 W/m-K
@Temperature 400 °C
hardened and tempered condition
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.28 %
Chromium, Cr 4.2 %
Cobalt, Co 8.5 %
Iron, Fe 71.52 %
Molybdenum, Mo 5.0 %
Tungsten, W 6.4 %
Vanadium, V 3.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels ASP 60 Cold Work Steel
Assab Steels ASP 23 Cold Work Steel
Crucible Steel Rex M2 High Speed Steel
AISI Type A2 Tool Steel
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C

NASSAB11 / 15029

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.