MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 4850.UV High Density Polyethylene Copolymer Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: ExxonMobil™ HD 4850.UV is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for articles requiring rugged physical performance in cold temperature environments

Availability: Latin America, North America and South America

Additive:

  • Long Term UV-15 Stabilizer: Yes
Applications:
  • Automotive Components
  • Industrial Closures
  • Recreation Vehicle – Components
  • Waste Carts

Information provided by ExxonMobil

Key Words: HDPE HD 6601.29
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ExxonMobil method
ESCR 10% Igepal® 20 hour20 hourF50; ASTM D1963B
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.4 MPa3400 psiASTM D638
Elongation at Break 1000 %1000 %
Flexural Modulus 0.965 GPa140 ksi2% Secant
Flexural Modulus, 1% Secant 1100 MPa160000 psiASTM D790B
Izod Impact, Notched 0.534 J/cm
@Temperature -40.0 °C
1.00 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 130 °C<= 266 °FPeak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 66.7 °C152 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.2 °C108 °FASTM D648B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene
ExxonMobil HD 6480.UV High Density Polyethylene Resin
Petromont 1202 High Density Polyethylene Resin
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE
Dow DMDA-8007 NT 7 High Density Polyethylene Resin

PEX99295 / 175531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.