MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ ES-96 One Component Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD Thermoset ES-96 adhesive is a white, one-component, heat cured epoxy adhesive featuring excellent thermal stability and rapid cure rates. Thermoset ES-96 adhesive exhibits minimal flow during cure and provides excellent resistance to acids and strong bases. This product is a modification of CK6150S with enhanced air release characteristics.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/cc
Density 12.9 lb/gal
Viscosity 145000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
@Temperature 125 °C
cured
 90
@Temperature 25.0 °C
cured
Shear Strength >= 1600 psiTensile Shear, AL-AL, cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
@Temperature 25.0 °C
cured
Dielectric Constant 3.9
@Frequency 1000 Hz,
Temperature 25.0 °C
cured
Dielectric Strength >= 500 V/milcured
Dissipation Factor 0.10
@Frequency 1000 Hz,
Temperature 25.0 °C
cured
 0.20
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured
 0.20
@Frequency 60 Hz,
Temperature 25.0 °C
cured
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.922 W/m-Kcured
Maximum Service Temperature, Air 180 °Cmaximum continual temperature, cured
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hour
@Temperature 177 °C
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
 0.500 hour
@Temperature 121 °C
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
Gel Time 1.00 min
@Temperature 177 °C
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
 10.0 min
@Temperature 121 °C
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
Shelf Life 3.00 Month
@Temperature 0.000 °C
 
Descriptive Properties
AppearanceWhite Thixotropic (Available in different colors)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9226 / 232582

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.