MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives Thermoset™ ES-96 One Component Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD Thermoset ES-96 adhesive is a white, one-component, heat cured epoxy adhesive featuring excellent thermal stability and rapid cure rates. Thermoset ES-96 adhesive exhibits minimal flow during cure and provides excellent resistance to acids and strong bases. This product is a modification of CK6150S with enhanced air release characteristics.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/cc
Density 1.55 g/cc0.0558 lb/in³
Viscosity 145000 cP145000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  70
@Temperature 125 °C
70
@Temperature 257 °F
cured
 90
@Temperature 25.0 °C
90
@Temperature 77.0 °F
cured
Shear Strength >= 11.0 MPa>= 1600 psiTensile Shear, AL-AL, cured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm
@Temperature 25.0 °C
>= 1.00e+15 ohm-cm
@Temperature 77.0 °F
cured
Dielectric Constant 3.9
@Frequency 1000 Hz,
Temperature 25.0 °C
3.9
@Frequency 1000 Hz,
Temperature 77.0 °F
cured
Dielectric Strength >= 19.7 kV/mm>= 500 kV/incured
Dissipation Factor  0.10
@Frequency 1000 Hz,
Temperature 25.0 °C
0.10
@Frequency 1000 Hz,
Temperature 77.0 °F
cured
 0.20
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.20
@Frequency 1e+6 Hz,
Temperature 77.0 °F
cured
 0.20
@Frequency 60 Hz,
Temperature 25.0 °C
0.20
@Frequency 60 Hz,
Temperature 77.0 °F
cured
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.922 W/m-K6.40 BTU-in/hr-ft²-°Fcured
Maximum Service Temperature, Air 180 °C356 °Fmaximum continual temperature, cured
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 177 °C
0.167 hour
@Temperature 351 °F
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
 30.0 min
@Temperature 121 °C
0.500 hour
@Temperature 250 °F
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
Gel Time  1.00 min
@Temperature 177 °C
1.00 min
@Temperature 351 °F
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
 10.0 min
@Temperature 121 °C
10.0 min
@Temperature 250 °F
ES-96 is designed for use in masses of <5 grams. Larger masses or excessive temperatures may lead to violent exothermic reactions.
Shelf Life 3.00 Month
@Temperature 0.000 °C
3.00 Month
@Temperature 32.0 °F
 
Descriptive Properties
AppearanceWhite Thixotropic (Available in different colors)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9226 / 232582

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.