MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® E-434 Polyether Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol E-434 polyether polyol is a 4,800-molecular-weight polyoxypropylene triol specially modified with ethylene oxide.

Properties / Applications: Because Arcol E-434 contains a high percentage of primary hydroxyl groups, it has a relatively high rate of reactivity. It is compatible with most polyether polyols and can be blended with other diols, triols and polymer polyols to achieve desirable modifications of product properties. Arcol E-434 polyol is used in elastomeric applications and in the production of high-resilience flexible and semi-rigid foams. Typical applications include sealants, caulks, deck coatings, elastomers, tire fill and reaction injection molding (RIM). As with any product, use of Arcol E-434 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
Bulk Density 1.03 g/cc0.0370 lb/in³
Viscosity 820 cP820 cP
Storage Temperature 15.0 - 60.0 °C59.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.015<= 0.015[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 191 °C376 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.070 %<= 0.070 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number33.8-37.2 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® F-1080 Polyol
Covestro Arcol® E-351 Polyether Polyol
Covestro Arcol® 700 Polyether Polyol
Covestro Arcol® 34-45 Polyether Polyol
Covestro Arcol® 34-28 Polyether Polyol

PCOVEST0019 / 201802

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.