MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and low-adhesion surfaces.

Performance Features:

  • Excellent hydrolysis resistance
  • High microbial resistance
  • High stability of melt
  • High production rates
  • Low-adhesion surfaces
Applications: For the production of jacket material for cables, jackets for high pressure hose spiral hoses, profiles

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
Melt Index of Compound 55 g/10 min
@Load 21.6 kg,
Temperature 190 °C
55 g/10 min
@Load 47.6 lb,
Temperature 374 °F
cm3/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiDIN 53504
Elongation at Break 500 %500 %DIN 53504
100% Modulus 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
DIN 53504
300% Modulus 16.0 MPa
@Strain 300 %
2320 psi
@Strain 300 %
DIN 53504
Rebound 33 %33 %Bayshore
Tear Strength 65.0 kN/m371 pliISO 34-1
Abrasion 3535mm3; ISO 4549
Compression Set  25 %
@Temperature 23.0 °C,
Time 86400 sec
25 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D395
 45 %
@Temperature 70.0 °C,
Time 86400 sec
45 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 171 °C320 - 340 °F
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Front Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °F
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
Lubrizol LifeSciences Tecophilic® HP-60D-20 Hydrophilic TPU – Extrusion Grade
Covestro Texin® DP7-1049 Thermoplastic Polyurethanes (TPU)

PHU9944 / 150404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.