MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3X3G5 BK 23187 25% Glass Filled PA66 FR (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: 25% glass-fiber reinforced injection molding grade with enhanced fire-protection properties and increased long-term stability containing red phosphorus as flame retardant; has outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.2 - 1.6 %1.2 - 1.6 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 5.7 - 6.3 %5.7 - 6.3 %ISO 62
Viscosity Measurement 140140ISO 307
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inrestricted
Melt Flow 53.6 g/10 min
@Load 5.00 kg,
Temperature 275 °C
53.6 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 6.00 GPa870 ksiISO 527-1/-2
Izod Impact, Notched (ISO) 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 3500 MPa
@Strain <=0.5 %
508000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.10
@Frequency 1e+6 Hz
0.10
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 V575 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.330 W/m-K2.29 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20000hr
 153 °C307 °Ffor 50% loss of tensile strength after 5000hr
 220 °C428 °F
Decomposition Temperature >= 310 °C>= 590 °F
Ignition Temperature >= 350 °C>= 662 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Zone 1 290 °C554 °FFeed Zone
Zone 2 290 °C554 °FCompression
Zone 3 290 °C554 °FMetering-zone
Zone 4 290 °C554 °FNozzle
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
 290 °C554 °FOptimal
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection-molding
 80.0 °C176 °FOptimal
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 23187
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG0310 / 131943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.