MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3X3G5 BK 23187 25% Glass Filled PA66 FR (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: 25% glass-fiber reinforced injection molding grade with enhanced fire-protection properties and increased long-term stability containing red phosphorus as flame retardant; has outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.34 g/ccISO 1183
Moisture Absorption at Equilibrium 1.2 - 1.6 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 5.7 - 6.3 %ISO 62
Viscosity Measurement 140ISO 307
Linear Mold Shrinkage 0.0050 cm/cmrestricted
Melt Flow 53.6 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 4.5 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 6.00 GPaISO 527-1/-2
Izod Impact, Notched (ISO) 17.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 3500 MPa
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.10
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.330 W/m-KDIN 52612
Melting Point 260 °CDIN 53765
Maximum Service Temperature, Air 135 °Cfor 50% loss of tensile strength after 20000hr
 153 °Cfor 50% loss of tensile strength after 5000hr
 220 °C
Decomposition Temperature >= 310 °C
Ignition Temperature >= 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Zone 1 290 °CFeed Zone
Zone 2 290 °CCompression
Zone 3 290 °CMetering-zone
Zone 4 290 °CNozzle
Melt Temperature 280 - 300 °CInjection-molding/Extrusion
 290 °COptimal
Mold Temperature 60.0 - 90.0 °CInjection-molding
 80.0 °COptimal
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 23187
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG0310 / 131943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.