MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC); Polycarbonate/ASA Alloy, Unreinforced

Material Notes: Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Moisture Absorption at Equilibrium 0.15 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.40 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cmISO 294-4
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 45 g/10 min
@Load 5.00 kg,
Temperature 260 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 120 MPaISO 2039-1
Tensile Strength, Yield 61.0 MPaISO 527
Elongation at Break 50 %ISO 527
Elongation at Yield 4.0 %ISO 527
Tensile Modulus 2600 MPaISO 527
Flexural Strength 90.0 MPaISO 178
Izod Impact, Notched 150 J/mASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0060
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 - 85.0 µm/m-°CISO 11359
Thermal Conductivity 0.190 W/m-KDIN 52612-1
 0.190 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 100 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 105 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 110 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 300 °CISO 294
Mold Temperature 80.0 °CISO 294
Injection Velocity 200 mm/secISO 294
Drying Temperature 85.0 - 95.0 °C
@Time 7200 - 14400 sec
 
Descriptive Properties
ColorBlack 89828
 Gray 48350
 Natural
 White 36925
 White 36975
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 570 NC000 POM-GF20
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry)
Covestro Makrolon® 9415(Z) Polycarbonate

PBASG0594 / 132227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.