MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP611R Phenolic Paper Laminate Sheet, NEMA XP
Categories: Polymer; Thermoset; Phenolic

Material Notes: A hot-punching, paper based phenolic grade. With mechanical properties approaching those of NP610, NP611R also offers improved electrical and punching characteristics. NP611R is a warm to hot punching grade, used for switch parts and other applications that need good moisture resistance, such as switch bases, terminal boards, insulating washers, and other intricate punched parts. NP611R complies with the requirements of MIL-I-24768/19, Type PBM-P.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA XP, MIL-I-24768/19 - PBM-P, ASTM D709 Type I Grade XP
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 1.50 %
@Thickness 1.57 mm
ASTM D570 Condition D1-24/23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100
@Thickness 6.35 mm
ASTM D785
Tensile Strength 13500 psi
@Thickness 3.17 mm
CrossWise; ASTM D638 Condition A
 18000 psi
@Thickness 3.17 mm
LengthWise; ASTM D638 Condition A
Flexural Strength 22000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 29000 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Flexural Modulus 900 ksi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 1200 ksi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 45000 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
Shear Strength 12200 psi
@Thickness 1.57 mm
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched 0.600 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 0.700 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 600 V/mil
@Thickness 1.57 mm
ASTM D149 Condition A
Dielectric Breakdown 4000 V
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
 50000 V
@Thickness 1.57 mm
ASTM D149 Condition A
Arc Resistance 75 sec
@Thickness 3.17 mm
ASTM D495 Conition A
Comparative Tracking Index 180 V
@Thickness 3.17 mm
ASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Thickness 3.17 mm
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 17.0 µm/m-°C
@Thickness 3.17 mm
IPC-TM 650-2.4.24
UL RTI, Electrical 130 °CUL Bulletin 746b
UL RTI, Mechanical with Impact 130 °CUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength1100[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta RTB320S Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta RTB320X Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta NP602 Phenolic Paper Laminate Sheet
Norplex-Micarta NP600 Phenolic Paper Laminate Sheet
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled

PNORPM006 / 192763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.