MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP611R Phenolic Paper Laminate Sheet, NEMA XP
Categories: Polymer; Thermoset; Phenolic

Material Notes: A hot-punching, paper based phenolic grade. With mechanical properties approaching those of NP610, NP611R also offers improved electrical and punching characteristics. NP611R is a warm to hot punching grade, used for switch parts and other applications that need good moisture resistance, such as switch bases, terminal boards, insulating washers, and other intricate punched parts. NP611R complies with the requirements of MIL-I-24768/19, Type PBM-P.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA XP, MIL-I-24768/19 - PBM-P, ASTM D709 Type I Grade XP
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc
@Thickness 12.7 mm
1.35 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 1.50 %
@Thickness 1.57 mm
1.50 %
@Thickness 0.0620 in
ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100
@Thickness 6.35 mm
100
@Thickness 0.250 in
ASTM D785
Tensile Strength  93.1 MPa
@Thickness 3.17 mm
13500 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 124 MPa
@Thickness 3.17 mm
18000 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  152 MPa
@Thickness 1.57 mm
22000 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 200 MPa
@Thickness 1.57 mm
29000 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Flexural Modulus  6.21 GPa
@Thickness 1.57 mm
900 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 8.27 GPa
@Thickness 1.57 mm
1200 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 310 MPa
@Thickness 12.7 mm
45000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Shear Strength 84.1 MPa
@Thickness 1.57 mm
12200 psi
@Thickness 0.0620 in
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched  0.320 J/cm
@Thickness 12.7 mm
0.600 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 0.374 J/cm
@Thickness 12.7 mm
0.700 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.6 kV/mm
@Thickness 1.57 mm
600 kV/in
@Thickness 0.0620 in
ASTM D149 Condition A
Dielectric Breakdown  4000 V
@Thickness 1.57 mm
4000 V
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 50000 V
@Thickness 1.57 mm
50000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Arc Resistance 75 sec
@Thickness 3.17 mm
75 sec
@Thickness 0.125 in
ASTM D495 Conition A
Comparative Tracking Index 180 V
@Thickness 3.17 mm
180 V
@Thickness 0.125 in
ASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Thickness 3.17 mm
7.22 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 17.0 µm/m-°C
@Thickness 3.17 mm
9.44 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
UL RTI, Electrical 130 °C266 °FUL Bulletin 746b
UL RTI, Mechanical with Impact 130 °C266 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength1100[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta RTB320S Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta RTB320X Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta NP602 Phenolic Paper Laminate Sheet
Norplex-Micarta NP600 Phenolic Paper Laminate Sheet
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled

PNORPM006 / 192763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.