High Density Ethylene Hexene Copolymer with Synthetic Antistat Customer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most benefits. Has excellent stiffness and exceptional ESCR. Applications: Bottles for bleach and detergents, industrial chemicals, industrial parts, pharmaceutical packaging. Processing Recommendations: Blow Molding Stock Temperature: Upper Limit: 204°C, Lower Limit: 171°C Extrusion Melt Temperature: Upper Limit: 216°C, Lower Limit: 194°C Thermoforming Surface Temperature: Upper Limit: 182°C, Lower Limit: 171°C Specification Data: ASTM D4976 - PE 235. ASTM D1248 -Type III, Class A, Category 5. FDA Regulation 177.1520. Suitable for food packaging applications. Suitable for Kosher food packaging. Listed in Drug Mater File. Sag Upper Limit: 18 cm, Lower Limit: 13 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature. Data provided by Chevron Phillips Chemical Company, LP. |