MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HHM 5502 BZ High Density Ethylene Hexene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: High Density Ethylene Hexene Copolymer

Customer Benefits: This resin eliminates the need for a mold release agent at machine side. Incorporation of zinc stearate at resin extrusion assures uniform, consistent release properties.

Applications: Injection blow molding

Processing Recommendations:
Melting Temperature: Upper Limit: 260°C, Lower Limit: 232°C

Specification Data: ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Category 5. FDA Regulation 177.1520(c)3.2. Suitable for food packaging. Limited to application temperatures of 100°C and below (Condition B-H, Table 2,21 CFR 176.170). Listed in Drug Master File

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D1505
Environmental Stress Crack Resistance 35 hour35 hourCondition B, F50
ESCR 100% Igepal® 45 hour45 hourCondition A, F50 (100% Igepal CO-630), ASTM D1693
Melt Flow 0.35 g/10 min0.35 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psi2 in per min; ASTM D638 Type IV
Elongation at Break >= 600 %>= 600 %2 in per min; ASTM D638 Type IV
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 - 260 °C450 - 500 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer
Equate EMDA-6147 HDPE Blow Molding Resin
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade

PCHEVM20 / 20310

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.