MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aclo Accutech Polypropylene CP0435G20CV Copolymer Glass Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Approved to GMP.PP.029

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D1238
Ash 18 - 22 %18 - 22 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength, Yield 46.0 MPa6670 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 2.20 GPa319 ksiASTM D638
Flexural Strength 60.0 MPa8700 psiASTM D790
Flexural Modulus 2.499 GPa362.5 ksiASTM D790
Izod Impact, Notched 2.30 J/cm4.30 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C240 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade
Aclo Accucomp Polypropylene CPO406L Copolymer
Aclo Accutech Polypropylene CP0435G20HIV Copolymer Glass Reinforced High Impact

PACLO085 / 22340

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.