MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS Tristar® PC-10GF-HC-V 10% Glass Fiber Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: 10% Glass Fiber Reinforced Polycarbonate with Release and UV. Non-Chlorine, Non Bromine FR system. Application: Parts requiring High stiffness, close tolerances. Keywords: UL 945VA, UL746H, RoHS.

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Water Absorption 0.12 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 62.0 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 15 %
@Thickness 3.17 mm
ASTM D638
Flexural Strength 96.5 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 3.10 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
ASTM D256
Tensile Impact Strength 53.3 kJ/m²
@Thickness 3.17 mm
ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+15 ohm-cm
@Treatment Temp. 90.0 °C,
Time 346000 sec
50% RH; ASTM D257
 6.00e+15 ohm-cm
@Treatment Temp. 23.0 °C,
Time 144000 sec
50% RH; ASTM D257
Dielectric Strength 19.0 kV/mm
@Thickness 3.00 mm
ASTM D149
Arc Resistance 0.00 - 60 secPLC 7
Comparative Tracking Index 175 - 250 VPLC3
Hot Wire Ignition, HWI 30 - 60 secPLC 2
High Amp Arc Ignition, HAI >= 120 arcsPLC 0
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minPLC 0
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 138 °CASTM D648
UL RTI, Electrical 80.0 °C
 125 °C
UL RTI, Mechanical with Impact 80.0 °C
 115 °C
UL RTI, Mechanical without Impact 80.0 °C
 125 °C
Flammability, UL94 V-0
@Thickness 3.00 mm
UL File # E155285
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 2.50 mm
UL File # E155285
 5VA
@Thickness 2.50 mm
UL File # E155285
 5VA
@Thickness 3.00 mm
UL File # E155285
Oxygen Index 37.1 %
Glow Wire Ignition Temperature 875 °C
Glow Wire Flammability Index 960 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 254 - 274 °C
Middle Barrel Temperature 266 - 277 °C
Front Barrel Temperature 277 - 293 °C
Nozzle Temperature 271 - 293 °C
Melt Temperature 282 - 304 °C
Mold Temperature 71.1 - 93.3 °Csurface
Drying Temperature 121 °C
@Time 14400 sec
Injection Pressure 75.8 - 124 MPa
Back Pressure 0.345 - 1.38 MPa
Clamp Pressure 27.6 - 68.9 MPa
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Injection SpeedEdge Gate=slow to medium
 Tab Gate=medium to fast
 Tunnel Gate= fast
Non-Bromine, Non-Chlorinepass, UL 746H
Processing Methodinjection molding
RoHS CompliancePass, UL 746R

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GF-HC 10% Glass Fiber Polycarbonate
Covestro Bayblend® FR3000 PC/ABS Blend
Avient Edgetek® PC-30GF/000 BLACK Polycarbonate (PC)
PTS Tristar® PC-06 6 MFI Extrusion Grade Polycarbonate
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release

PZ9PT93c / 198157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.