MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HP561X Film Grade Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen HP561X is new generation Melt-Blown grade of Pellet type made by “New process and catalyst technology. Moplen HP561X shows better processing, color and thermal stability than general Melt-Blown grade of flake type. Moplen HP561X has narrow MWD, this product is typically used in Diaper and Air filter applications high barrier properties are required

Product Features: Excellent Spinnability /Excellent Drawability -Lower shot and fly & Higher MB web strength /Higher productivity /Convenient handling, Pellet type /Very good barrier property - Higher hydrohead value /Good processing, color and thermal stability /Good electrocharge property

Typical Applications: Diaper and Sanitary Napkin with Spunbond/Oil Absorbent Mat/Wipers/Air Filtration Media/Masks/Wet tissues/Base resin for color master batch

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 800 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen HP461X Melt-Blown Grade Polypropylene
PolyMirae Moplen HP461Y Melt-Blown Grade Polypropylene
Braskem CP1200B Homopolymer Polypropylene
PolyMirae Moplen HF461X Fiber (Melt-blown) Grade Polypropylene
Borealis BJ356MO Polypropylene Copolymer

PMIRAF44 / 183265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.