MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen HP461Y Melt-Blown Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Moplen HP461Y is new generation Melt-Blown grade of Pellet type made by “New process and catalyst technology". Moplen HP461Y shows better processing, color and thermal stability than general Melt-Blown grade of flake type. Moplen HP461Y has narrow MWD, this product is typically used in Diaper and Air filter applications high barrier properties are required.

Product Features: Excellent Spinnability /Excellent Drawability -Lower shot and fly & Higher MB web strength /Higher productivity /Convenient handling, Pellet type /Very good barrier property - Higher hydrohead value /Good processing, color and thermal stability /Good electrocharge property /Low processing temperature(Energy cost saving effect)

Typical Applications: Diaper and Sanitary Napkin with Spunbond/Oil Absorbent Mat/Wipers/Air Filtration Media/Wet tissues/Base resin for color master batch

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 1300 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1300 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen HP561X Film Grade Polypropylene
PolyMirae Moplen HP461X Melt-Blown Grade Polypropylene
Braskem CP1200B Homopolymer Polypropylene
Braskem H 152 Fiber Extrusion Polypropylene
Braskem Evateno® HM 150 EVA Hot Melt Copolymer

PMIRAF39 / 183260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.