MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dover Chemical DOVERPHOS 53 Tri (C12-14) alkyl Phosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos 53 is tri (C12-14) alkyl phosphite. The molecular weight and phosphorus content of Doverphos 53 is intermediate among the alkyl phosphites. Doverphos 53 can be used as a stabilizer for PVC, LLDPE, HDPE, and other polymers. Typical use levels range from 0.10 to 2.00%.

Information provided by DoverChem

Key Words: CAS# 68610-62-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.872 - 0.882 g/cc
@Temperature 25.0 °C
0.872 - 0.882 g/cc
@Temperature 77.0 °F
ASTM D1298
ASTM Color <= 50<= 50APHA; ASTM D1209
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10[mgKOH/gm]; ASTM D3242
 
Thermal PropertiesMetricEnglishComments
Melting Point 25.0 °C77.0 °FProduct may freeze during cold storage
 
Optical PropertiesMetricEnglishComments
Refractive Index <= 1.4595
@Temperature 25.0 °C
<= 1.4595
@Temperature 77.0 °F
ASTM D1218

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® Seal-Fit PA6/66 (Dry)

WDOVER043 / 217662

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.