Doverphos 53 is tri (C12-14) alkyl phosphite. The molecular weight and phosphorus content of Doverphos 53 is intermediate among the alkyl phosphites. Doverphos 53 can be used as a stabilizer for PVC, LLDPE, HDPE, and other polymers. Typical use levels range from 0.10 to 2.00%.Information provided by DoverChem |