MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel strengths along with good impact and durability. It bonds extremely well to many surfaces. It also has lower odor when compared to traditional fast cure epoxies and acrylic adhesives. It is formulated for low halogen content.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 6500 cPAccelerator, RVF #7 spindle, 20 rpm
 11000 cPBase, RVF #7 spindle, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 28.0 psiOverlap HDPE
 88.0 psiOverlap, Polyacrylic
 280 psiOverlap, Polycarbonate
 350 psiOverlap, ABS
 2140 psiOverlap, Galvanized Steel Hot dipped
 2200 psiOverlap, Aluminum MEK/abrade/MEK
 2200 psiOverlap, CRS MEK/abrade/MEK
 4650 psiEtched Aluminum Overlap, Methyl Ethyl Ketone, RT for 30 days immersion
 5140 psiEtched Aluminum Overlap, Water Vapor 66°C, 80% RH for 14 days
 5530 psiOverlap, Aluminum Etched
 5530 psiEtched Aluminum Overlap, RT/50% RH for 14 days
 3500 psi
@Temperature -55.0 °C
Aluminum Overlap
 5300 psi
@Temperature 23.0 °C
Aluminum Overlap
 850 psi
@Temperature 82.0 °C,
Time 900 sec
Aluminum Overlap
 1890 psi
@Time 14400 sec
Aluminum Overlap
Peel Strength 11.0 pli
@Temperature 82.0 °C
Aluminum, Bell Peel
 15.0 pli
@Temperature -55.0 °C
Aluminum, Bell Peel
 21.0 pli
@Temperature 23.0 °C
Aluminum, Bell Peel
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 minTime to Handling Strength
 
Descriptive Properties
AppearanceClear
 Off-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP405 Black Epoxy Adhesive
Solvay METLBOND® 1515-4 Epoxy Film Adhesive
Lord Adhesives 6100 Silver Conductor
ASTM A525 Galvanized Steel
Armstrong X-81-A/F Epoxy Adhesive

PMM34641 / 169388

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.