(Viewing data as-entered.
Click here
to return)
Morgan Advanced Ceramics AL-995™ Alumina
Categories:
Ceramic
;
Oxide
;
Aluminum Oxide
Material Notes:
Exceptional mechanical, thermal, electrical, and chemical properties. High purity grades that can also be used for metallized applications.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
3.75
-
3.95
g/cc
Fired
Porosity
0.00 %
Apparent, fully dense grades
Particle Size
1.0
-
12
µm
Grain size
Mechanical Properties
Original Value
Comments
Hardness, Rockwell 45 N
81 - 86
Vickers Microhardness
14300 - 18500
MPa, at Hv 0.5kg
Modulus of Elasticity
370
-
400
GPa
@Temperature 20.0 °C
Flexural Strength
310
-
500
MPa
@Temperature 20.0 °C
3-point
Compressive Strength
2000
-
2500
MPa
Fracture Toughness
4.00
MPa-m½
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+7
-
6.00e+8
ohm-cm
@Temperature 600 °C
1.00e+14
-
1.00e+17
ohm-cm
@Temperature 20.0 °C
Dielectric Constant
9.3
@Frequency 1e+9 Hz
9.7 - 10
@Frequency 9.40e+9 Hz
9.7 - 10.1
@Frequency 1e+6 Hz
Dielectric Strength
20.0
-
31.5
kV/mm
@Thickness 2.00 - 3.00 mm,
Temperature 20.0 °C
DC
Dissipation Factor
0.00014
@Frequency 1e+9 Hz
Dielectric Loss Index
0.00029
@Frequency 1e+7 Hz
K*tan delta
0.00050 - 0.00080
@Frequency 1e+6 Hz
0.00050 - 0.0010
@Frequency 9.40e+9 Hz
0.00084
@Frequency 8.50e+9 Hz
K*tan delta
0.0013
@Frequency 1e+9 Hz
K*tan delta
Thermal Properties
Original Value
Comments
CTE, linear
6.90
-
8.90
µm/m-°C
@Temperature 20.0 °C
8.50
-
9.00
µm/m-°C
@Temperature 800 °C
Specific Heat Capacity
0.880
J/g-°C
Thermal Conductivity
12.5
W/m-K
@Temperature 400 °C
25.6
-
30.0
W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air
1500
-
1725
°C
Component Elements Properties
Original Value
Comments
Al2O3
99.5 %
Descriptive Properties
Te Value
975
°C
Thermal Downshock
160-210
Change in °C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Morgan Advanced Ceramics AL-300™ 97-99% Alumina
Astro Met AmAlOx 87 Alumina - Aluminum Oxide
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Overview of materials for Gray Cast Iron
Morgan Advanced Ceramics Deranox™ 999 >99% Alumina
CMORG20 / 90398
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.