MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Deranox™ 999 >99% Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Exceptional mechanical, thermal, electrical, and chemical properties. High purity grades that can also be used for metallized applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.75 - 3.95 g/cc0.135 - 0.143 lb/in³Fired
Porosity 0.00 %0.00 %Apparent, fully dense grades
Particle Size 1.0 - 12 µm1.0 - 12 µmGrain size
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 81 - 8681 - 86
Vickers Microhardness 14300 - 1850014300 - 18500MPa, at Hv 0.5kg
Modulus of Elasticity 370 - 400 GPa
@Temperature 20.0 °C
53700 - 58000 ksi
@Temperature 68.0 °F
Flexural Strength 310 - 500 MPa
@Temperature 20.0 °C
45000 - 72500 psi
@Temperature 68.0 °F
3-point
Compressive Strength 2000 - 2500 MPa290000 - 363000 psi
Fracture Toughness 4.00 MPa-m½3.64 ksi-in½
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.00e+7 - 6.00e+8 ohm-cm
@Temperature 600 °C
1.00e+7 - 6.00e+8 ohm-cm
@Temperature 1110 °F
 1.00e+14 - 1.00e+17 ohm-cm
@Temperature 20.0 °C
1.00e+14 - 1.00e+17 ohm-cm
@Temperature 68.0 °F
Dielectric Constant  9.3
@Frequency 1e+9 Hz
9.3
@Frequency 1e+9 Hz
 9.7 - 10
@Frequency 9.40e+9 Hz
9.7 - 10
@Frequency 9.40e+9 Hz
 9.7 - 10.1
@Frequency 1e+6 Hz
9.7 - 10.1
@Frequency 1e+6 Hz
Dielectric Strength 20.0 - 31.5 kV/mm
@Thickness 2.00 - 3.00 mm,
Temperature 20.0 °C
508 - 800 kV/in
@Thickness 0.0787 - 0.118 in,
Temperature 68.0 °F
DC
Dissipation Factor 0.00014
@Frequency 1e+9 Hz
0.00014
@Frequency 1e+9 Hz
Dielectric Loss Index  0.00029
@Frequency 1e+7 Hz
0.00029
@Frequency 1e+7 Hz
K*tan delta
 0.00050 - 0.00080
@Frequency 1e+6 Hz
0.00050 - 0.00080
@Frequency 1e+6 Hz
 0.00050 - 0.0010
@Frequency 9.40e+9 Hz
0.00050 - 0.0010
@Frequency 9.40e+9 Hz
 0.00084
@Frequency 8.50e+9 Hz
0.00084
@Frequency 8.50e+9 Hz
K*tan delta
 0.0013
@Frequency 1e+9 Hz
0.0013
@Frequency 1e+9 Hz
K*tan delta
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.90 - 8.90 µm/m-°C
@Temperature 20.0 °C
3.83 - 4.94 µin/in-°F
@Temperature 68.0 °F
 8.50 - 9.00 µm/m-°C
@Temperature 800 °C
4.72 - 5.00 µin/in-°F
@Temperature 1470 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°F
Thermal Conductivity  12.5 W/m-K
@Temperature 400 °C
86.8 BTU-in/hr-ft²-°F
@Temperature 752 °F
 25.6 - 30.0 W/m-K
@Temperature 20.0 °C
178 - 208 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1500 - 1725 °C2730 - 3137 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.9 %99.9 %
 
Descriptive Properties
Te Value975°C
Thermal Downshock160-210Change in °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Deranox™ 970 Mac-A970R Aluminum Oxide Ceramic
Morgan Advanced Ceramics Deranox™ 970 Alumina
Morgan Advanced Ceramics Deranox™ 970 97-99% Alumina
Morgan Advanced Ceramics Deranox™ 975 Alumina
Morgan Advanced Ceramics Deranox™ 975 Mac-A975R Aluminum Oxide Ceramic

CMORG24 / 90402

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.