MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC) Coated Polyester Film

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccAverage value: 1.40 g/cc Grade Count:10
Moisture Vapor Transmission 0.00800 - 0.200 cc-mm/m²-24hr-atmAverage value: 0.110 cc-mm/m²-24hr-atm Grade Count:10
Water Vapor Transmission 0.600 - 9.00 g/m²/dayAverage value: 6.12 g/m²/day Grade Count:10
Oxygen Transmission 0.00210 - 0.200 cc-mm/m²-24hr-atmAverage value: 0.109 cc-mm/m²-24hr-atm Grade Count:10
Thickness 12.7 - 25.0 micronsAverage value: 18.2 microns Grade Count:10
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 100 - 170 %Average value: 129 % Grade Count:10
Film Elongation at Break, TD 70.0 - 140 %Average value: 89.5 % Grade Count:10
Modulus of Elasticity 3.45 - 3.79 GPaAverage value: 3.55 GPa Grade Count:10
Tear Strength Test 300 - 500Average value: 365 Grade Count:10
Seal Strength 156 - 201 g/25 mmAverage value: 188 g/25 mm Grade Count:7
Film Tensile Strength at Break, MD 152 - 186 MPaAverage value: 172 MPa Grade Count:10
Film Tensile Strength at Break, TD 179 - 248 MPaAverage value: 217 MPa Grade Count:10
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CAverage value: 121 °C Grade Count:10
 
Optical PropertiesOriginal ValueComments
Haze 2.50 - 8.00 %Average value: 6.56 % Grade Count:8
Gloss 130 - 200 %Average value: 150 % Grade Count:8
Transmission, Visible 70.0 - 90.0 %Average value: 82.9 % Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyvinyl Dichloride (PVDC)
Overview of materials for PVC, Molded
Overview of materials for High Density Polyethylene (HDPE), Film Grade
SK Chemicals Saran® 168
SK Chemicals Saran® 506 Polymer

O5101 / 78471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.