MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Lupolen 4261 A IM High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Lupolen 4261 A IM is a high molecular weight high density polyethylene. Typical customer applications include components for automotive fuel tank applications. It is supplied in pelletized form and is stabilized with antioxidants for the injection molding process. The product features an outstanding Environmental Stress Cracking Resistance (ESCR), good chemical resistance in combination with an excellent low temperature impact resistance. Typical process includes injection molding. Lupolen 4261 A IM is not intended for use in medical and pharmaceutical applications. Applications: Fuel Tanks, Non-fuel Reservoirs

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.940 g/cc0.0340 lb/in³ISO 1183-1
Melt Flow 15 g/10 min
@Load 21.6 kg,
Temperature 190 °C
15 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.0 MPa3050 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 0.800 GPa116 ksiISO 527-1,-2
Tensile Impact Strength 140 kJ/m²
@Temperature -30.0 °C
66.6 ft-lb/in²
@Temperature -22.0 °F
notched, type 1, method A; ISO 8256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FISO 3146
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 280 °C446 - 536 °F
 
Descriptive Properties
FNCT (hrs)35ISO 16770, 3.5 MPa, 2% Arkopal N100, 80°C
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Entec Hypel® PEHD20/.953 HDPE
Envalior Pocan® B 3235 + 000000 PBT, 30% Glass Fiber Reinforced
LyondellBasell Alathon M 5265 High Denisty Polyethylene
LyondellBasell Alathon® M4612 High Density Polyethylene
LyondellBasell Alathon® M5562 High Density Polyethylene

PEQT8562 / 220197

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.