MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon M 5265 High Denisty Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Alathon high density polyethylene resins are produced in North America using slurry and solution technologies and include bi-modal HMW grades commonly used in pressure pipe and blown film, general purpose and thin-wall injection molding grades, and blown film grades known for their moisture barrier performance.

Alathon M5265 is a narrow molecular weight distribution octene-copolymer used in the manufacture of open-head pails and covers. Applications: Containers, Pails.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.593 - 0.625 g/cc0.0214 - 0.0226 lb/in³ASTM D1895
Density 0.951 g/cc0.0344 lb/in³ASTM D1505
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 19.6 cm7.72 inLYB Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171D 2240
Tensile Strength at Break >= 27.6 MPa>= 4000 psiASTM D638
Tensile Strength, Yield 26.4 MPa3830 psiASTM D638
Elongation at Break >= 2230 %>= 2230 %ASTM D638
Elongation at Yield 12 %12 %ASTM D638
Modulus of Elasticity 0.765 GPa111 ksiASTM D790
Tensile Modulus 0.681 GPa98.8 ksi1% secant; ASTM D638
Flexural Modulus, 1% Secant 1130 MPa164000 psiASTM D790
2% Secant Modulus 0.945 GPa137 ksiASTM D790
Izod Impact, Notched 0.640 J/cm
@Temperature 23.0 °C
1.20 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
@Temperature -18.0 °C
NB
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 131.7 °C269.1 °FASTM D3418
Crystallization Temperature 117.8 °C244.0 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 69.4 °C157 °Funannealed; ASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D 746
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon M 6080UV High Denisty Polyethylene
LyondellBasell Alathon® M5562 High Density Polyethylene
LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded
Aclo Accutech Polyethylene HD0204UVL High Density UV Stabilized
Aclo Accucomp Polyethylene HD0205L High Density

PEQT7065 / 218703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.