MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Arnite® AV2 390 XL PET GF50
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 50% Glass Reinforced

Material Notes: 50% Glass Reinforced, Low outgassing

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/ccISO 1183
Water Absorption 0.30 %Sim. To ISO 62
Moisture Absorption 0.120 %Sim. To ISO 62
Viscosity 20000 cP
@Shear Rate 100000 1/s,
Temperature 295 °C
 23000 cP
@Shear Rate 100000 1/s,
Temperature 315 °C
 30000 cP
@Shear Rate 100000 1/s,
Temperature 270 °C
 200000 cP
@Shear Rate 1000 1/s,
Temperature 295 °C
 230000 cP
@Shear Rate 1000 1/s,
Temperature 315 °C
 300000 cP
@Shear Rate 1000 1/s,
Temperature 270 °C
Linear Mold Shrinkage, Flow 0.0045 cm/cmSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmSim. To ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 210 MPaISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
Tensile Modulus 19.0 GPaISO 527-1/-2
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.011
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 35.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 252 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.47 mm
IEC 60695-11-10
 HB
@Thickness 0.810 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Arnite® AV2 390 XT PET GF50
Envalior Arnite® AV2 370 XT PET-GF35
Envalior Arnite® A04 900 PET (European Grade)
Envalior Arnite® AV2 370 XL PET-GF35
Envalior Arnite® AV2 370 HF PET-GF35

PDSM9795 / 161416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.