MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Arnite® AV2 370 XL PET-GF35
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 40% Glass Reinforced

Material Notes: 35% Glass Reinforced, Low Outgassing

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³ISO 1183
Water Absorption 0.45 %0.45 %Sim. To ISO 62
Moisture Absorption 0.180 %0.180 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 185 MPa26800 psiISO 527-1/-2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 13.0 GPa1890 ksiISO 527-1/-2
Charpy Impact Unnotched  6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
 3.7
@Frequency 100 Hz
3.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm838 kV/inIEC 60243-1
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
IEC 60250
 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnite® AV2 370 XT PET-GF35
Envalior Arnite® AV2 370 XL-T PET-GF35
Envalior Arnite® AV2 370 HF PET-GF35
Envalior Arnite® AV2 390 XL PET GF50
Envalior Arnite® AV2 390 XT PET GF50

PDSM9798 / 161419

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.